High temperature oxidation behaviour of single crystal superalloys RR3000 and CMSX-4

CM Younes, GC Allen, JA Nicholson

Research output: Contribution to journalArticle (Academic Journal)peer-review

24 Citations (Scopus)
Translated title of the contributionHigh temperature oxidation behaviour of single crystal superalloys RR3000 and CMSX-4
Original languageEnglish
Pages (from-to)80 - 88
Number of pages9
JournalCorrosion Engineering, Science and Technology
Volume42 (1)
DOIs
Publication statusPublished - Mar 2007