Micro-fractography of cleavage fracture by EBSP technology and computer assisted stereophotogrammetry

  • COA Semprimoschnig
  • , R Rippan
  • , O Kolednik
  • , DJ Dingley

Research output: Chapter in Book/Report/Conference proceeding › Conference Contribution (Conference Proceeding)

Translated title of the contributionMicro-fractography of cleavage fracture by EBSP technology and computer assisted stereophotogrammetry
Original languageEnglish
Title of host publicationMechanisms and Mechanics of Damage and Failure, Proc. of 11th Biennial Eur. Conf. on Fracture ECF 11 Eng. Mater. Advisory Services
Pages753 - 758
Volume1
Publication statusPublished - 1996

Cite this