Surface Analysis of Titanium Implants

  • GC Allen
  • , DS Sutherland
  • , PD Forshaw
  • , IT Brown
  • , KR Williams

Research output: Contribution to journalArticle (Academic Journal)peer-review

72 Citations (Scopus)
Translated title of the contributionSurface Analysis of Titanium Implants
Original languageEnglish
Pages (from-to)893 - 899
Number of pages6
JournalBiomaterials
Volume14
Publication statusPublished - 1993